Can you make that allergy claim?

The allergy label is a marketing word with a legal shadow. What you can say depends on the market, and the safest claim is usually the most specific one.

Published 2026-11-23 · Reviewed by Felix, founder of KUBO Jewelry

Stainless steel earrings and rings shown against a plain background
The claim that survives scrutiny is specific: grade, plus test, plus report number.
Short answer

Stainless steel is not free of nickel, and allergy claims on 304 or 316L are risky in all major markets. In the EU, nickel release from items in prolonged skin contact is restricted under REACH, demonstrated by testing to EN 1811. In the US the FTC requires such claims to be substantiated. The defensible claim is grade plus test report.

The label sells. The label also invites a complaint you cannot answer, because the allergy claim carries no numeric definition in most markets. Specific claims — a grade, a standard, a report number — are both safer and more persuasive to a professional buyer, and they cost nothing to write.

What the EU requires

Nickel release from articles in prolonged skin contact is restricted under the EU's REACH Regulation, and compliance is demonstrated on the finished article, not on the raw steel.

Compliance is shown by testing the finished piece to EN 1811, the reference method for nickel release, with EN 12472 used for coated items to simulate wear before the release test. The release limit sits at 0.5 µg/cm² per week for items in prolonged contact, and roughly half that for piercing posts. A 3 g stud and a 30 g bangle sit under the same threshold — what changes between them is the surface area, not the limit.

Two consequences for a brand:

  • The finished piece is what is tested, not the raw steel. A mill certificate proves the grade; it does not satisfy the release requirement.
  • Coated pieces are tested after simulated wear, which is exactly the scenario a customer creates by wearing the ring daily.

Enforcement sits with ECHA and the market surveillance authorities of the member states, and in practice a complaint from a consumer association or a retailer is the usual trigger. By the time the letter arrives, the only useful document is a test report that already exists.

What the UK and US require

The UK retains the EU's nickel restrictions in domestic law, so a piece compliant for the EU is generally compliant for the UK. The US is different: there is no mandatory release threshold for jewelry in the same way, but any health-related claim must be substantiated before it is made.

The FTC's Jewelry Guides, published at 16 CFR Part 23, require exactly that substantiation, and a claim the data would contradict is not a claim — it is a liability. California adds a second layer: OEHHA maintains the Proposition 65 list, and nickel appears on it, which is why some listings carry a warning label. Our guide to Proposition 65 and jewelry covers what triggers a warning and how the label is worded.

So "zero nickel" on a stainless steel product is a claim you would have to defend with data, and the data would contradict it.

Words to retire

Four claims appear on product pages every week, and none of them survives a professional buyer's second question.

ClaimProblem
Zero-nickelFalse for 304 and 316L — typical mill ranges run 8–10.5% nickel for 304 and 10–14% for 316L
Allergy-safeA medical claim with no defined test behind it
Dermatologist-testedNo named protocol, no report, no number
Surgical steelNot a recognised grade; it means nothing and excludes nothing

The pattern across all four is the same: each asserts an outcome without naming the evidence. A buyer who asks "tested to what, by whom, against which limit" gets no answer, and a buyer who has been asked that question by their own regulator stops asking politely.

Words that work

Three constructions put something checkable in the sentence, which is what a serious retail buyer wants:

  • "316L stainless steel, a molybdenum-bearing grade chosen for corrosion resistance."
  • "Nickel release tested to EN 1811 by a third-party lab — report number on request."
  • "PVD-coated stainless steel; the finished piece is tested as worn, to EN 1811 with EN 12472."

Each is checkable, and checkable is what a merchandiser who has been burned by a claim prefers to any adjective. Note also what the third construction does not say: a coating is not a barrier claim, because the test that governs is run on the finished piece after wear, not on the coating in isolation.

The practical sequence

Five steps take a brand from assumption to a claim it can defend:

  1. Specify 316L for anything in prolonged skin contact.
  2. Get a mill certificate for the steel — it proves the grade, not the release.
  3. Test one finished piece per construction and finish — typically 3–5 pieces across a first collection, since the test is per construction rather than per design.
  4. Put the report number in your product data.
  5. Write care and material copy around the grade, not around a guarantee.

Testing costs a few hundred dollars per construction and typically takes 10–20 days of lab time including the wear simulation, and it is per construction rather than per design. It is the cheapest credibility a jewelry brand can buy.

Our guide to nickel release under REACH covers the test method in detail. Pieces in prolonged contact — earrings with posts, rings worn every day — are where the testing earns its keep, and a material and test plan can be written into the order through the RFQ page.

Next step

Have a project this applies to?

Minimum order 100 pcs per design.